GC Analysis of Bleed Profiles of GC Septa on SLB®-5ms

GC Analysis of Bleed Profiles of GC Septa on SLB®-5ms

Conditions

column SLB-5ms, 30 m x 0.25 mm I.D., 0.25 µm (28471-U)
oven 40 C (3 min), 15 C/min to 325 C (15 min)
carrier gas helium, 25 cm/sec constant
sample solvent extracts of septa, dodecane (as an internal standard) added to 100 µg/mL
injection 1 muLsplitless (1 min)
liner 4 mm I.D., single taper, unpacked
inj. temp. 250 C
detector FID, 325 C

Description

Categories Analytical Chromatography, GC Applications, Volatiles
Featured Industry General Analytical
Legal Information SLB is a registered trademark of Sigma-Aldrich Co. LLC
Other Notes Complementary products:
Syringes
Vials
Gas Purification and Gas Management
Inlet Liners, Glass Wool, and Specialized Hand Tools
Septa and Specialized Hand Tools
Column Ferrules, Nuts, and Specialized Hand Tools
suitability application for GC

Materials

     
Related Links