GC Analysis of Fluorocarbons on Alumina Chloride PLOT

GC Analysis of Fluorocarbons on Alumina Chloride PLOT

Conditions

column Alumina Chloride PLOT, 50m x 0.53mm ID, 10mum (28329-U)
oven 35 C (1.0 min), 12 C/min to 180 C
carrier gas helium, 3.0 ml/min
sample Freons @ ~20% each (custom standard)
injection 10 µl
inj. temp. 200 C
detector FID, 230C

Description

Categories Analytical Chromatography, GC Applications, Gases
Featured Industry Chemicals and Industrial Polymers
suitability application for GC

Analyte

  • Dichlorofluoromethane
  • Freon 11
  • Freon 114
  • Freon 114a
  • Freon 12
  • Freon 21
  • Freon 22
  • Trichlorofluoromethane

Materials

     