Literature suggests that the following materials can be used to prepare MIL-88B(2OH). 

Applications

When constructed with:

Fe, Cr

  • Gas adsorption
  • Separations
  • Catalysis

Properties

When constructed with:

Fe, Cr

  • Cell Volume =  2800 Å3

 

Materials

     

References

  1. Horcajada, P.; Salles, F.; Wuttke, S.; Devic, T.; Heurtaux, D.; Maurin, G.; Vimont, A.; Daturi, M.; David, O.; Magnier, E.; Stock, N.; Filinchuk, Y.; Popov, D.; Riekel, C.; Ferey, G.; Serre, C. J. Am. Chem. Soc. 2011, 133, 17839-17847.

 