porph@MOM-10 Supplemental Information

Explore MOF Applications, Properties and Materials to construct MOFs in the MOF Constructor Tool

 

Literature suggests that the following materials can be used to prepare porph@MOM-10. 

Applications

  • Chemical Synthesis

Properties

  • Two types of square channels = (A) 12.6 Å × 12.6 Å; (B) 11.9 Å × 11.9 Å