Tantalum

foil, thickness 0.25 mm, ≥99.9% trace metals basis

Sinônimo(s):
Ta
Empirical Formula (Hill Notation):
Ta
Número CAS:
Peso molecular:
180.95
Número EC:
Número MDL:
ID de substância PubChem:
NACRES:
NA.23

Nível de qualidade

100

pressão de vapor

<0.01 mmHg ( 537.2 °C)

teor

≥99.9% trace metals basis

forma

foil

temperatura de autoignição

572 °F

resistividade

13.5 μΩ-cm, 20°C

espessura

0.25 mm

pb

5425 °C (lit.)

pf

2996 °C (lit.)

densidade

16.69 g/cm3 (lit.)

SMILES string

[Ta]

InChI

1S/Ta

InChI key

GUVRBAGPIYLISA-UHFFFAOYSA-N

Categorias relacionadas

Descrição geral

The structure of tantalum is body centered cubic (BCC) metal. It is a refractory metal; stable up to very high temperatures. Tantalum is ductile at room temperature and moderately ductile at cryogenic temperatures. Compton profile of highly pure thin elemental foil of tantalum was investigated using IGP type coaxial photon detector.1

Embalagem

100 cm2 in rigid mailer

Quantidade

50x50 mm (approximately 10.4 g)
100x100 mm (approximately 41.6 g)

Storage Class Code

13 - Non Combustible Solids

WGK Alemanha

nwg

Ponto de fulgor (ºF)

Not applicable

Ponto de fulgor (ºC)

Not applicable

Equipamento de proteção individual

Eyeshields, Gloves, type N95 (US)

Certificado de análise

Certificado de origem

The Morphology of Tensile Failure in Tantalum
Boyce BL, et al.
Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 44(10), 4567-4580 (2013)
Scott M Sporer et al.
Clinical orthopaedics and related research, 470(11), 3156-3163 (2012-09-25)
Stabilization of a pelvic discontinuity with a posterior column plate with or without an associated acetabular cage sometimes results in persistent micromotion across the discontinuity with late fatigue failure and component loosening. Acetabular distraction offers an alternative technique for reconstruction...
Thomas Larzon et al.
Vascular, 21(2), 87-91 (2013-03-20)
Control of back bleeding from the hypogastric artery into the aneurysm after endovascular aneurysm repair (EVAR) of a ruptured aorto-iliac aneurysm may be necessary in order to avoid a type II endoleak. It is an emergency situation and selective catheterization...
Orbital ultrasound in the selective screening of a dural-cavernous sinus fistula.
Hamid Shokoohi et al.
European journal of emergency medicine : official journal of the European Society for Emergency Medicine, 20(2), 137-139 (2013-02-26)
Stuart A Callary et al.
Clinical orthopaedics and related research, 471(7), 2238-2244 (2013-01-22)
One cross-linked polyethylene (XLPE) liner is manufactured using a lower dose of radiation, 5 Mrad, which may result in less cross-linking. The reported in vivo wear rate of this XLPE liner in patients undergoing THA has varied, and has included...

Artigos

Biomedical Implant Devices Fabricated from Low Young’s Modulus Titanium Alloys Demonstrating High Mechanical Biocompatibility

Biomedical implants are essentially foreign substances within the human body that must survive many years’ exposure to demanding mechanical and physiological conditions. Despite these challenges, metal implants have been widely used to substitute for or rebuild hard tissues such as bones and teeth.

Nossa equipe de cientistas tem experiência em todas as áreas de pesquisa, incluindo Life Sciences, ciência de materiais, síntese química, cromatografia, química analítica e muitas outras.

Entre em contato com a assistência técnica