ログインで組織・契約価格をご覧ください。
サイズを選択してください
現在、価格および在庫状況を閲覧できません。
この商品について
実験式(ヒル表記法):
Zn
CAS番号:
分子量:
65.39
NACRES:
NA.23
PubChem Substance ID:
UNSPSC Code:
12141750
MDL number:
スキップする
製品名
亜鉛, foil, 8mm disks, thickness 0.01mm, 99.9%
InChI
1S/Zn
SMILES string
[Zn]
InChI key
HCHKCACWOHOZIP-UHFFFAOYSA-N
vapor pressure
1 mmHg ( 487 °C)
assay
≥99.9%
form
foil
manufacturer/tradename
Goodfellow 102-817-21
resistivity
5.8 μΩ-cm, 20°C
bp
907 °C (lit.)
mp
420 °C (lit.)
density
7.133 g/mL at 25 °C (lit.)
1 of 4
当該品目 | GF07065255 | GF23081835 | GF87282254 |
|---|---|---|---|
| form foil | form foil | form foil | form foil |
| assay ≥99.9% | assay 99.9% | assay 99.90% | assay ≥99.9% |
| manufacturer/tradename Goodfellow 102-817-21 | manufacturer/tradename Goodfellow 070-652-55 | manufacturer/tradename Goodfellow 230-818-35 | manufacturer/tradename Goodfellow 872-822-54 |
| resistivity 5.8 μΩ-cm, 20°C | resistivity 5.8 μΩ-cm, 20°C | resistivity 5.8 μΩ-cm, 20°C | resistivity 5.8 μΩ-cm, 20°C |
| density 7.133 g/mL at 25 °C (lit.) | density 7.133 g/mL at 25 °C (lit.) | density 7.133 g/mL at 25 °C (lit.) | density 7.133 g/mL at 25 °C (lit.) |
| bp 907 °C (lit.) | bp 907 °C (lit.) | bp 907 °C (lit.) | bp 907 °C (lit.) |
Legal Information
Goodfellow製品
General description
For updated SDS information please visit www.goodfellow.com.
Tandra Ghoshal et al.
Journal of nanoscience and nanotechnology, 9(9), 5586-5591 (2009-11-26)
Nanowire arrays of zinc oxide were synthesized on zinc foil by a simple thermal evaporation process. Morphologies and sizes of the synthesized nanostructures were varied by varying the reaction time and the surface roughness of the substrate. Self-catalytic liquid-solid mechanism
Chenglin Yan et al.
The journal of physical chemistry. B, 110(51), 25850-25855 (2006-12-22)
Vertically aligned ZnO nanorods with uniform diameter and length have been synthesized on a zinc foil substrate with ammonium persulfate as oxidant via a facile, larger scale production and inexpensively synthesized method without any templates or additives. SEM and XRD
A new vapor-phase hydrothermal method to concurrently grow ZnO nanotube and nanorod array films on different sides of a zinc foil substrate.
Haimin Zhang et al.
Chemistry (Weinheim an der Bergstrasse, Germany), 18(17), 5165-5169 (2012-03-21)
S Rondot et al.
Science (New York, N.Y.), 263(5154), 1739-1741 (1994-03-25)
An x-ray projection microscope equipped with a charge-coupled device camera allows direct observation of zinc (Zn(2+)) ions diffusing in aqueous hydrochloric acid solution during the corrosion of zinc foil and pellets. Time series of microradiographic images with a lateral resolution
Xufeng Wu et al.
Chemical communications (Cambridge, England), (15)(15), 1655-1657 (2006-04-04)
Highly oriented ZnO nanoneedle/nanorods arrays have been fabricated by direct oxidation of zinc foil in alkaline zincate ion solution at near room temperature (20 degrees C for nanoneedles, 30 degrees C for nanorods).