ログインで組織・契約価格をご覧ください。
この商品について
実験式(ヒル表記法):
Zn
CAS番号:
分子量:
65.39
NACRES:
NA.23
PubChem Substance ID:
UNSPSC Code:
12141750
MDL number:
スキップする
製品名
亜鉛, foil, 5m coil, thickness 0.15mm, as rolled, 99.95+%
InChI
1S/Zn
SMILES string
[Zn]
InChI key
HCHKCACWOHOZIP-UHFFFAOYSA-N
vapor pressure
1 mmHg ( 487 °C)
assay
99.95%
form
foil
manufacturer/tradename
Goodfellow 265-009-35
resistivity
5.8 μΩ-cm, 20°C
L × thickness
5 m × 0.15 mm
bp
907 °C (lit.)
mp
420 °C (lit.)
density
7.133 g/mL at 25 °C (lit.)
1 of 4
当該品目 | GF66475390 | GF49751781 | GF91311869 |
|---|---|---|---|
| manufacturer/tradename Goodfellow 265-009-35 | manufacturer/tradename Goodfellow 664-753-90 | manufacturer/tradename Goodfellow 497-517-81 | manufacturer/tradename Goodfellow 913-118-69 |
| form foil | form foil | form foil | form foil |
| assay 99.95% | assay 99.95% | assay 99.95% | assay ≥99.95% |
| resistivity 5.8 μΩ-cm, 20°C | resistivity 5.8 μΩ-cm, 20°C | resistivity 5.8 μΩ-cm, 20°C | resistivity 5.8 μΩ-cm, 20°C |
| density 7.133 g/mL at 25 °C (lit.) | density 7.133 g/mL at 25 °C (lit.) | density 7.133 g/mL at 25 °C (lit.) | density 7.133 g/mL at 25 °C (lit.) |
| bp 907 °C (lit.) | bp 907 °C (lit.) | bp 907 °C (lit.) | bp 907 °C (lit.) |
Legal Information
Goodfellow製品
General description
For updated SDS information please visit www.goodfellow.com.
A new vapor-phase hydrothermal method to concurrently grow ZnO nanotube and nanorod array films on different sides of a zinc foil substrate.
Haimin Zhang et al.
Chemistry (Weinheim an der Bergstrasse, Germany), 18(17), 5165-5169 (2012-03-21)
Chenglin Yan et al.
The journal of physical chemistry. B, 110(51), 25850-25855 (2006-12-22)
Vertically aligned ZnO nanorods with uniform diameter and length have been synthesized on a zinc foil substrate with ammonium persulfate as oxidant via a facile, larger scale production and inexpensively synthesized method without any templates or additives. SEM and XRD
Zhonghao Li et al.
Chemical communications (Cambridge, England), (41)(41), 6273-6275 (2009-10-15)
Aligned ZnO arrays with branched rods, hexagonal rods, quasi-round rods, hexagonal pyramids and porous nanostructures are constructed on zinc foil in the ionic liquid tetrabutylammonium hydroxide aqueous solution.
Chuanhui Xia et al.
Journal of nanoscience and nanotechnology, 11(12), 10506-10510 (2012-03-14)
We have investigated the properties of Mn-doped ZnO nanocrystalline film growing on zinc foil by the hydrothermal method. X-ray photoelectron spectroscopy shows that the manganese ions exist as Mn2+ in the film. From UV-vis spectra, we observe a red shift
Tandra Ghoshal et al.
Nanotechnology, 19(6), 065606-065606 (2008-02-13)
ZnO nanowire arrays were synthesized on zinc foil by a simple thermal evaporation process at relatively low temperature. Morphology and size controlled synthesis of the ZnO nanostructures was achieved by variation of the synthesis temperature, reaction time and the surface
アクティブなフィルタ
ライフサイエンス、有機合成、材料科学、クロマトグラフィー、分析など、あらゆる分野の研究に経験のあるメンバーがおります。.
製品に関するお問い合わせはこちら(テクニカルサービス)