378496

Sigma-Aldrich

Poly(methylphenylsiloxane)

viscosity 450-550 cSt 

Linear Formula:
-Si(CH3)(C6H5)O-n
CAS Number:
MDL number:
PubChem Substance ID:
NACRES:
NA.23
Pricing and availability is not currently available.

refractive index

n20/D 1.5365 (lit.)

viscosity

450-550 cSt(25 °C)
450-550 cSt

density

1.102 g/mL at 25 °C (lit.)

Related Categories

Personal Protective Equipment

dust mask type N95 (US),Eyeshields,Gloves

RIDADR

NONH for all modes of transport

WGK Germany

WGK 3

Flash Point(F)

437.0 °F - closed cup

Flash Point(C)

225.00 °C - closed cup

H Kriegs et al.
The Journal of chemical physics, 124(10), 104901-104901 (2006-03-18)
In some polymers, in addition to the usual structural alpha relaxation, a slower alpha' relaxation is observed with a non-Arrhenius temperature dependence. In order to understand better the molecular origin of this alpha' relaxation in poly(methylphenylsiloxane) (PMPS) we have studied...
Experience with a silicone resin (polymethylphenylsiloxane) hard contact lens.
H Magatani et al.
The CLAO journal : official publication of the Contact Lens Association of Ophthalmologists, Inc, 9(3), 261-266 (1983-07-01)
O Gyllenhaal et al.
Journal of chromatography, 516(2), 415-426 (1990-09-21)
The supercritical fluid chromatography of intact aliphatic amines with different columns is described. One group of amines was based on N,N-dimethyl-n-octylamine and related primary and secondary amines, and the other on the amino alcohol metoprolol and several of its analogues....
Janka Mydlová-Memersheimerová et al.
Journal of chromatography. A, 1216(32), 6043-6062 (2009-07-11)
The gas chromatographic-mass spectrometric (GC-MS) separation of all 209 polychlorinated biphenyl (PCB) congeners was studied on an extremely efficient 80 m x 0.1mm i.d. capillary column coated with a 0.1 microm film of poly(5%-phenyl methyl)siloxane stationary phase. The quality of...
G B Chen et al.
Se pu = Chinese journal of chromatography, 18(4), 343-345 (2003-01-25)
An insoluble beta-cyclodextrin polymer cross-linked with epichlorohydrin was prepared. beta-Cyclodextrin polymer (0.26 g) was treated for 0.5 h by a ultrasonator in the mixed solvent (10 mL) of isopropyl ether, methylene dichloride and benzene with a volume ratio 2:1:2, and...

Our team of scientists has experience in all areas of research including Life Science, Material Science, Chemical Synthesis, Chromatography, Analytical and many others.

Contact Technical Service

Social Media

LinkedIn icon
Twitter icon
Facebook Icon
Instagram Icon

MilliporeSigma

Research. Development. Production.

We are a leading supplier to the global Life Science industry with solutions and services for research, biotechnology development and production, and pharmaceutical drug therapy development and production.

© 2021 Merck KGaA, Darmstadt, Germany and/or its affiliates. All Rights Reserved.

Reproduction of any materials from the site is strictly forbidden without permission.