Co3(BHTC)2 Supplemental Information

Explore MOF Applications, Properties and Materials to construct MOFs in the MOF Constructor Tool

 

Literature suggests that the following materials can be used to prepare Co3(BHTC)2

Applications

  • Separations
  • Catalysis

Properties

  • Maximum Surface Area: 1300 m2 / g Langmuir Surface Area

 