CPM-18-Sm Supplemental Information

Explore MOF Applications, Properties and Materials to construct MOFs in the MOF Constructor Tool

 

Literature suggests that the following materials can be used to prepare CPM-18-Sm. 

Applications

When constructed with:

In, Sm

  • Gas adsorption:  Hydrogen, nitrogen, carbon dioxide gas

Materials

     