Proteins, DNA, lectins and many other species have been coupled to microparticles. Coupling to microparticles may be achieved by passive adsorption or covalent attachment. Most techniques using passive adsorption technology report four to six months of bead stability. This technology is the basis for most commercialized latex assays. The passively-bound proteins may eventually are lost from the surface of the particle. Some applications demand covalent techniques. Two major areas include materials with low affinity for polystyrene and cases where a component of the assay will displace passively adsorbed material. Many attempts to couple DNA have been successful only with covalent coupling or with a covalently coupled linking group. Surfactant is a notorious example of a material that can displace proteins from the bead’s surface. If surfactant is required as an additive in the assay, covalent coupling procedures are recommended.
For 0.5 mL of an aqueous 2.5% microparticle suspension, 200-400 micrograms protein and 1 mL 0.2 M ethanolamine in PBS are used.
Amino functional beads couple proteins with glutaraldehyde: Glutaraldehyde is more stable than the carbodiimide reagents used with carboxylate beads. Coupling with glutaraldehyde results in the proteins being bound 11-12 carbon atoms away from the surface of the bead versus 2-3 carbon atoms as in the case of carboxylate beads coupled using carbodiimide.
Protein Coupling Troubleshooting: |
---|