Accéder au contenu
MilliporeSigma

283622

Nickel(II) hydroxide

Synonyme(s) :

Nickel dihydroxide, Nickelous hydroxide

Se connecter pour consulter vos tarifs contractuels et ceux de votre entreprise/organisme

Sélectionner une taille de conditionnement

250 G

125,00 $

1 KG

400,00 $

125,00 $


Veuillez contacter notre Service Clients pour connaître la disponibilité de ce produit.

Demander une commande groupée

A propos de cet article

Formule linéaire :
Ni(OH)2
Numéro CAS:
Poids moléculaire :
92.71
Numéro CE :
Numéro MDL:
Code UNSPSC :
12352302
ID de substance PubChem :
Nomenclature NACRES :
NA.23

Passer à

Service technique
Besoin d'aide ? Notre équipe de scientifiques expérimentés est là pour vous.
Laissez-nous vous aider

Forme

powder

Pertinence de la réaction

core: nickel

Concentration

60.0-70.0% Ni (EDTA titration)

Pf

230 °C (lit.)

Densité

4.1 g/mL (lit.)

Application(s)

battery precursors
catalysts
material synthesis precursor

Chaîne SMILES 

O[Ni]O

InChI

1S/Ni.2H2O/h;2*1H2/q+2;;/p-2

Clé InChI

BFDHFSHZJLFAMC-UHFFFAOYSA-L

Vous recherchez des produits similaires ? Visite Guide de comparaison des produits

Comparer avec des articles similaires

Voir la comparaison complète

Montrer les différences

1 of 4

Cet article
544183561142451193
form

powder

form

powder

form

powder

form

powder

Quality Level

200

Quality Level

100

Quality Level

100

Quality Level

200

grade

reference material

grade

-

grade

anhydrous

grade

anhydrous

mp

230 °C (lit.)

mp

-

mp

963 °C (lit.)

mp

-

density

4.1 g/mL (lit.)

density

-

density

5.098 g/mL at 25 °C (lit.)

density

3.55 g/mL at 25 °C (lit.)

concentration

60.0-70.0% Ni (EDTA titration)

concentration

-

concentration

-

concentration

-

Application

Nickel hydroxide was used as a reference material in a study where the influence of stacking faults on the electrochemical activity of Ni(OH)2 electrodes was studied.[1]

Pictogrammes

Health hazardExclamation markEnvironment

Mention d'avertissement

Danger

Classification des risques

Acute Tox. 4 Inhalation - Acute Tox. 4 Oral - Aquatic Acute 1 - Aquatic Chronic 1 - Carc. 1A Inhalation - Muta. 2 - Repr. 1B - Resp. Sens. 1 - Skin Irrit. 2 - Skin Sens. 1 - STOT RE 1 Inhalation

Organes cibles

Lungs

Code de la classe de stockage

6.1D - Non-combustible acute toxic Cat.3 / toxic hazardous materials or hazardous materials causing chronic effects

Classe de danger pour l'eau (WGK)

WGK 3

Point d'éclair (°F)

Not applicable

Point d'éclair (°C)

Not applicable

Équipement de protection individuelle

Eyeshields, Faceshields, Gloves, type P3 (EN 143) respirator cartridges


Faites votre choix parmi les versions les plus récentes :

Certificats d'analyse (COA)

Lot/Batch Number

Vous ne trouvez pas la bonne version ?

Si vous avez besoin d'une version particulière, vous pouvez rechercher un certificat spécifique par le numéro de lot.

Déjà en possession de ce produit ?

Retrouvez la documentation relative aux produits que vous avez récemment achetés dans la Bibliothèque de documents.

Consulter la Bibliothèque de documents

Binder-free and full electrical-addressing free-standing nanosheets with carbon nanotube fabrics for electrochemical applications.
Tae Il Lee et al.
Advanced materials (Deerfield Beach, Fla.), 23(40), 4711-4715 (2011-09-14)
S Junaid S Qazi et al.
Journal of colloid and interface science, 348(1), 80-84 (2010-05-15)
Experimental evidence for the existence of 'cubatic' order in a colloidal dispersion of plate-like particles is presented. In a 'cubatic' phase, disk-like particles self-assemble with domains of a few parallel plates and the director tends to be orthogonal in adjacent
Baojun Li et al.
Chemical communications (Cambridge, England), 46(34), 6267-6269 (2010-07-29)
Mesoporous beta-Ni(OH)(2) synthesized by a soft template method as a cathode material in a nickel based battery can provide higher specific discharge capacity in comparison with other micro/nanostructures.
Sougata Sarkar et al.
Inorganic chemistry, 49(19), 8813-8827 (2010-09-10)
A surfactantless, trouble-free, and gentle wet chemistry approach has been used to interpret the precisely controlled growth of β-Ni(OH)(2) with the assistance of ammonia and nickel acetate from seedless mild hydrothermal conditions. A thorough investigation of the reaction kinetics and
Huaqiang Cao et al.
Chemphyschem : a European journal of chemical physics and physical chemistry, 11(2), 489-494 (2009-12-10)
Constructing complex nanostructures has become increasingly important in the development of hydrogen storage, self-cleaning materials, and the formation of chiral branched nanowires. Several approaches have been developed to generate complex nanostructures, which have led to novel applications. Combining biology and

Articles

Lithium-ion batteries' characteristics make them popular for electricity storage due to portability, rechargeability, and low cost.

The prevailing strategies for heat and electric-power production that rely on fossil and fission fuels are having a negative impact on the environment and on our living conditions.

Plasmonic nanoparticles have unique optical properties that can be tailored to suit a variety of applications in the biotechnology1–8 and electronics9–16 industries.

Questions

1–2 of 2 Questions  
  1. How can I determine the shelf life / expiration / retest date of this product?

    1 answer
    1. If this product has an expiration or retest date, it will be shown on the Certificate of Analysis (COA, CofA). If there is no retest or expiration date listed on the product's COA, we do not have suitable stability data to determine a shelf life. For these products, the only date on the COA will be the release date; a retest, expiration, or use-by-date will not be displayed.
      For all products, we recommend handling per defined conditions as printed in our product literature and website product descriptions. We recommend that products should be routinely inspected by customers to ensure they perform as expected.
      For products without retest or expiration dates, our standard warranty of 1 year from the date of shipment is applicable.
      For more information, please refer to the Product Dating Information document: https://www.sigmaaldrich.com/deepweb/assets/sigmaaldrich/marketing/global/documents/418/501/product-dating-information-06-25-mk.pdf

      Helpful?

  2. How is shipping temperature determined? And how is it related to the product storage temperature?

    1 answer
    1. Products may be shipped at a different temperature than the recommended long-term storage temperature. If the product quality is sensitive to short-term exposure to conditions other than the recommended long-term storage, it will be shipped on wet or dry-ice. If the product quality is NOT affected by short-term exposure to conditions other than the recommended long-term storage, it will be shipped at ambient temperature. As shipping routes are configured for minimum transit times, shipping at ambient temperature helps control shipping costs for our customers. For more information, please refer to the Storage and Transport Conditions document: https://www.sigmaaldrich.com/deepweb/assets/sigmaaldrich/marketing/global/documents/316/622/storage-transport-conditions-mk.pdf

      Helpful?

Reviews

No rating value

Active Filters

Notre équipe de scientifiques dispose d'une expérience dans tous les secteurs de la recherche, notamment en sciences de la vie, science des matériaux, synthèse chimique, chromatographie, analyse et dans de nombreux autres domaines..

Contacter notre Service technique