PM2547050

PTFE Membrane Filter, 2.0 μm Pore Size

Fluoropore®, filter diam. 46.2 mm, hydrophobic

Synonym(s):

PTFE for PM2.5 Particle Monitoring, PTFE, hydrophobic, 2.0 µm, 47 mm, white, plain, polypropylene ring, sequential serial number

Sign In to View Organizational & Contract Pricing.

Select a Size

Change View
Size/SKUAvailabilityPrice

About This Item

UNSPSC Code:
40161507
NACRES:
NB.24
eCl@ss:
32031602
Pore size:
2.0 μm pore size
Material:
PTFE membrane, plain filter, white filter
Feature:
hydrophobic
Diam.:
46.2 mm
Sterility:
non-sterile
Pricing and availability is not currently available.
Technical Service
Need help? Our team of experienced scientists is here for you.
Let Us Assist


Quality Segment

material

PTFE membrane, plain filter, white filter

sterility

non-sterile

feature

hydrophobic

manufacturer/tradename

Fluoropore®, Millipore

diam.

46.2 mm

filter diam.

46.2 mm

thickness

40 μm

matrix

Fluoropore®

pore size

2.0 μm pore size

shipped in

ambient

General description

Filter Type: Screen filter
Particulates and contaminants in the air affect human capital, the most precious natural resource. Recognizing the need to protect this resource, industries, governments and regulatory agencies around the world monitor ambient air. Millipore′s PTFE Membrane for PM2.5 Particle Monitoring has been developed using US EPA test standards.

Application

PM 2.5 particle monitoring

Legal Information

Fluoropore is a registered trademark of Merck KGaA, Darmstadt, Germany




Choose from one of the most recent versions:

Certificates of Analysis (COA)

Lot/Batch Number

It looks like we've run into a problem, but you can still download Certificates of Analysis from our Documents section.

If you need assistance, please contact Customer Support

Already Own This Product?

Find documentation for the products that you have recently purchased in the Document Library.

Visit the Document Library



Questions

Reviews

No rating value

Active Filters