Cationic Polymers HPLC on TSKgel® PWXL-CP Columns

Conditions | |
|---|---|
| column | TSKgel G3000PWXL-CP, 30 cm x 7.8 mm, 7 µm particles (821873) |
| column | TSKgel G6000PWXL-CP, 30 cm x 7.8 mm, 13 µm particles (821875) |
| column | TSKgel G5000PWXL-CP, 30 cm x 7.8 mm, 10 µm particles (821874) |
| column temp. | 25 °C |
| mobile phase | 0.1 M sodium nitrate |
| flow rate | 1 mL/min |
| sample | 3 mg/mL |
| injection | 100 µL |
| detector | refractive index (RI) |
Description | |
|---|---|
| Analysis Note | Various cationic polymers with different functional groups and molecular weights were injected on the TSKgel PWXL-CP columns (TSKgel G6000PWXL-CP, G5000PWXL-CP and G3000PWXL-CP, connected in series). |
| Categories | Analytical Chromatography, Polymers, coatings, and plastics |
| Featured Industry | Chemicals and Industrial Polymers |
| Other Notes | Data provided by Tosoh Bioscience LLC. |
| suitability | application for HPLC |
Materials
Sorry, an unexpected error has occurred
Response not successful: Received status code 500
Sign In To Continue
To continue reading please sign in or create an account.
Don't Have An Account?