GC Analysis of a 7-Component Sulfur Gases Mix on Supel-Q PLOT after SPME using 75 μm Carboxen/PDMS Fiber suitable for GC, application for SPME

Materials

related product

Product No.
Description
Pricing

Supel-Q PLOT Capillary GC Column

L × I.D. 30 m × 0.32 mm, average thickness 15 μm

used together

Product No.
Description
Pricing

SPME Fiber Assembly

75 μm CAR/PDMS, Fused Silica (1 cm), needle size 24 ga, Manual Holder, pk of 3, black hub

CONDITIONS

sample/matrix

sulfur gases in 40 mL vial

SPME fiber

Carboxen/PDMS, 75 μm (57318)

extraction

10 min headspace at 40 °C

desorption process

3 min at 290 °C

column

Supel-Q PLOT, 30 m × 0.32 mm I.D. (24242)

oven

45 °C (1 min) to 250 °C at 15 °C/min

detector

FPD